China Cheap price China N48 Customer Strong Magnetic Ainico NdFeB Magnet with Assembly&Pot

Short Description:

AlNiCo alloys basically consist of aluminum, nickel, cobalt, copper, iron and titanium. In some grades cobalt and/or titanium can be omitted. Also these alloys may contain additions of silicon, columbium, zirconium or other elements which enhance heat treatment response of one of the magnetic characteristics.  AlNiCo alloys are formed by casting or powder metallurgical processes.


Product Detail

Product Tags

We have been ready to share our knowledge of internet marketing worldwide and recommend you suitable merchandise at most aggressive rates. So Profi Tools present you very best price of money and we are ready to develop alongside one another with China Cheap price China N48 Customer Strong Magnetic Ainico NdFeB Magnet with Assembly&Pot, Our Lab now is “National Lab of diesel engine turbo technology ” , and we own a qualified R&D staff and complete testing facility.
We have been ready to share our knowledge of internet marketing worldwide and recommend you suitable merchandise at most aggressive rates. So Profi Tools present you very best price of money and we are ready to develop alongside one another with China Pot Magnet, Permanent Magnet, We have been increasingly expanding our international market share based on quality products and solutions, excellent service, reasonable price and timely delivery. Remember to contact us at any time for more information.
Introduction:
AlNiCo alloys basically consist of aluminum, nickel, cobalt, copper, iron and titanium. In some grades cobalt and/or titanium can be omitted. Also these alloys may contain additions of silicon, columbium, zirconium or other elements which enhance heat treatment response of one of the magnetic characteristics.  AlNiCo alloys are formed by casting or powder metallurgical processes.
Feature:
1. AlNiCo magnet has high remanent induction but low coercivity. It works stable at extreme temperature, maintaining its magnetic characteristics between –250ºC and 550ºC.  Based on superior magnetic induction, it is largely used in measuring equipment and detection systems.
2. Alnico is a fragile material and can only be altered during the casting process. Orientation of it achieved during heat treatment, producing a magnetic field with the defined magnetization direction.
3. Due to the low coercive force, AlNiCo magnets can be easily affected by reverse magnetic force and impact of iron. That’s why they can be easily demagnetized by external influences. For this reason, AlNiCo magnets should not be stored and packed with the same poles opposing to each other.
4. In open circuit, the ration of length/diameter (L/D) should be at least 4:1. With shorter length,
5. AlNiCo magnets behave well against oxidation. No coating required for surface protection.
Applications:
Use in high sensitivity products such as Instruments, Meters, Mobile Phones, Automobile parts, Electroacoustic devices, Motors, Teaching and Aerospace military, etc.
All stated values were determined using standard samples according IEC 60404-5. The following specifications serve as reference values and may differ.

Cast AlNiCo Magnet Physical Properties
Material Grade Remanence Rev. Temp.-Coeff. Of Br Coercivity Rev. Temp.-Coeff. Of Hcj Max. Energy  Product Max. Operating Temperature Density
Br (KGs) Hcb (KOe) (BH)max.  (MGOe) g/cm³
Isotropic LN9 6.8 -0.03 0.38 -0.02 1.13 450℃ 6.9
Isotropic LN10 6.0 -0.03 0.50 -0.02 1.20 450℃ 6.9
Isotropic LNG12 7.2 -0.03 0.50 +0.02 1.55 450℃ 7.0
Isotropic LNG13 7.0 -0.03 0.60 +0.02 1.60 450℃ 7.0
Isotropic LNGT18 5.8 -0.025 1.25 +0.02 2.20 550℃ 7.3
Anisotropic LNG37 12.0 -0.02 0.60 +0.02 1.65 525℃ 7.3
Anisotropic LNG40 12.5 -0.02 0.60 +0.02 5.00 525℃ 7.3
Anisotropic LNG44 12.5 -0.02 0.65 +0.02 5.50 525℃ 7.3
Anisotropic LNG52 13.0 -0.02 0.70 +0.02 6.50 525℃ 7.3
Anisotropic LNG60 13.5 -0.02 0.74 +0.02 7.50 525℃ 7.3
Anisotropic LNGT28 10.8 -0.02 0.72 +0.03 3.50 525℃ 7.3
Anisotropic LNGT36J 7.0 -0.025 1.75 +0.02 4.50 550℃ 7.3
Anisotropic LNGT32 8.0 -0.025 1.25 +0.02 4.00 550℃ 7.3
Anisotropic LNGT40 8.0 -0.025 1.38 +0.02 5.00 550℃ 7.3
Anisotropic LNGT60 9.0 -0.025 1.38 +0.02 7.50 550℃ 7.3
Anisotropic LNGT72 10.5 -0.025 1.40 +0.02 9.00 550℃ 7.3

 

Sintered AlNiCo Magnet Physical Properties
Material Grade Remanence Rev. Temp.-Coeff. Of Br Coercivity Coercivity Rev. Temp.-Coeff. Of Hcj Max. Energy Product Max. Operating Temperature Density
Br (KGs) Hcb (KA/m) Hcj (KA/m) (BH)max. (KJ/m³) g/cm³
Isotropic SALNICO4/1 8.7-8.9 -0.02 9-11 10-12 -0.03~0.03 3.2-4.8 750℃ 6.8
Isotropic SALNICO8/5 5.3-6.2 -0.02 45-50 47-52 -0.03~0.03 8.5-9.5 750℃ 6.8
Isotropic SALNICO10/5 6.3-7.0 -0.02 48-56 50-58 -0.03~0.03 9.5-11.0 780℃ 6.8
Isotropic SALNICO12/5 7.0-7.5 -0.02 50-56 53-58 -0.03~0.03 11.0-13.0 800℃ 7
Isotropic SALNICO14/5 7.3-8.0 -0.02 47-50 50-53 -0.03~0.03 13.0-15.0 790℃ 7.1
Isotropic SALNICO14/6 6.2-8.1 -0.02 56-64 58-66 -0.03~0.03 14.0-16.0 790℃ 7.1
Isotropic SALNICO14/8 5.5-6.1 -0.01 75-88 80-92 -0.03~0.03 14.0-16.0 850℃ 7.1
Isotropic SALNICO18/10 5.7-6.2 -0.01 92-100 99-107 -0.03~0.03 16.0-19.0 860℃ 7.2
Anisotropic SALNICO35/5 11-12 -0.02 48-52 50-54 -0.03~0.03 35.0-39.0 850℃ 7.2
Anisotropic SALNICO29/6 9.7-10.9 -0.02 58-64 60-66 -0.03~0.03 29.0-33.0 860℃ 7.2
Anisotropic SALNICO32/10 7.7-8.7 -0.01 90-104 94-109 -0.03~0.03 33.0-38.0 860℃ 7.2
Anisotropic SALNICO33/11 7.0-8.0 -0.01 107-115 111-119 -0.03~0.03 33.0-38.0 860℃ 7.2
Anisotropic SALNICO39/12 8.3-9.0 -0.01 115-123 119-127 -0.03~0.03 39.0-43.0 860℃ 7.25
Anisotropic SALNICO44/12 9.0-9.5 -0.01 119-127 124-132 -0.03~0.03 44.0-48.0 860℃ 7.25
Anisotropic SALNICO37/15 7.0-8.0 -0.1 143-151 150-158 -0.03~0.03 37.0-41.0 870℃ 7.2

Note:
· We remain the same as above unless specified from customer. Curie temperature and temperature coefficient are for reference only, not as a basis for decision.
· The maximum working temperature of magnet is changeable due to ratio of length and diameter and environment factors.


  • Previous:
  • Next:

  • Write your message here and send it to us